Hong-Chul Jeong 6 Articles
2032003
Development of Welding Flux to Reduce Hydrogen Embrittlement in Weld Zone
Sunghoon Chung, Il Sohn, Hong-Chul Jeong
J Weld Join. 2019;37(1):15-20.   Published online February 20, 2019
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Quantitative Analysis on the Effects of Welding Parameters on Diffusible Hydrogen Contents in Weld Metal Produced by FCAW Process
Dong-Woo Han, Kook-Soo Bang, Hong-Chul Jeong, Jong-Bong Lee
J Weld Join. 2010;28(2):54-59.   Published online May 13, 2010
PDFPDF    
Recent Development and Welding Properties of High Strength Hot Rolled Steels for Lifting, Handling and Transport Equipments
Young-Roc Im, Chang-Hoon Lee, Jung-Chul Lee, Hong-Chul Jeong
J Weld Join. 2009;27(2):19-26.   Published online May 18, 2009
PDFPDF    
Recent Development of Structural Steel and Its Weldability for Construction
Hong-Chul Jeong, Jin-Woo Lee
J Weld Join. 2009;27(1):49-58.   Published online March 12, 2009
PDFPDF    
Mechanical Properties and Microstructures of High Heat Input Welded Tandem EGW Joint in EH36-TM Steel
Hong-Chul Jeong, Young-Hwan Park, Young-Ho An, Jong-Bong Lee
J Weld Join. 2007;25(1):57-62.   Published online March 26, 2007
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI